Area of Application:
Suitable for welding Q & T high tensile steel type HY 130 and equalient normalized - tempered fine grain structural
Chemical Properties:
Carbon: 0.10%, Manganese: 1.20-1.80%, Silicon: 0.30-0.60%, Sulfur: 0.025%, Phosphorus: 0.025%, Chromium: 0.70-0.90%, Molybdenum: 0.50-0.70%, Nickel: 2.00-2.60%, Vanadium: 0.50%
Mechanical Properties:
Tensile Strength: 830 min, Yield Strength: 740 min, Elongation: 14 min, Charpy Impact: 70-140 Joules